The rapid expansion of the use of Li-ion batteries (LIBs) across diverse applications, from portable electronics to battery electric vehicles and large-scale energy storage systems, underscores the need to better understand and to improve their performance, longevity, and safety. An in-depth understanding of LIB degradation processes is essential for developing advanced operating profiles to enlarge their lifetime. This is not only crucial for maximizing sustainability but also for reducing costs simultaneously. Furthermore, ensuring cell safety over the full lifespan even under diverse and extreme operating conditions is critical. This requires a detailed understanding and identification of factors such as deposition of metallic Li that causes rapid battery aging and compromises safety. LIB degradation is driven by numerous factors. They can be grouped into material and design aspects as well as operating and storage conditions. Among these, temperature is one of the most significant influencing factors on LIB degradation. At low temperatures (often < 25 °C), Li plating typically dominates degradation, while at elevated temperatures accelerated parasitic side reactions such as solid-electrolyte-interphase (SEI) growth are dominant. Both mechanisms result in significantly different safety characteristics. Finding the optimal temperature is a trade-off between both aging mechanisms. This thesis focuses on investigations of temperature dependent aging mechanisms in LIBs using various methods of investigation. Results were reported in the following seven peer-reviewed articles. In the first article, the impact of operating conditions such as temperature, current, and aging state on LIB degradation is examined by using cylindrical 21700-type cells as well as lab-made pouch cells. Arrhenius plots of the cyclic aging rate are used to determine the crossover temperature between Li plating at low temperatures and SEI growth at high temperatures. It is shown that both, aging state and C-rate, shift the crossover temperature. Particularly higher charging C-rates shift the onset of Li plating and thus the crossover temperature towards higher values. In typical applications, the operating temperature of a battery is not constant but fluctuates in between certain limits. However, most scientific investigations focus on aging processes at one constant temperature only. In the second article, the effect of varying temperatures during cyclic aging is examined. Results reveal that the initial aging temperature can substantially alter subsequent degradation behavior. Especially, aging at high temperatures shifts the onset of Li plating to lower temperatures in subsequent cycles. As a consequence, the optimal aging temperature is reduced and cycle life is extended. Conversely, cycling LIBs under conditions that support Li plating accelerates further Li plating. The materials choice, particularly on the anode side, further affects the temperature dependent performance. Si-graphite composites are used as anode material in state-of-the-art LIBs. However, Si and graphite have a significantly different electrochemical behavior. The effect of a varying Si content on the temperature dependent performance and degradation is investigated in the third article. A high Si content in the anode is beneficial for a good low temperature performance. However, the high temperature performance is deteriorated by a high Si content due to a strongly increasing cyclic aging rate. Therefore, a balanced Si content in the anode is essential to optimize both, cycle life and performance. Li deposition in LIBs is problematic, as it correlates with rapid capacity fade and safety concerns. In the fourth article, three workflows addressing whether Li deposition exists in a cell, its location, and the conditions that prevent its formation are presented. Complementary experimental techniques as well as simulation approaches to detect and prevent Li deposition are reviewed. The workflows enable accurate and efficient detection of Li deposition and provide valuable insights for improving battery design, safety, and performance in demanding applications. Safety of LIBs is significantly influenced by their aging history. In the fifth article, the influence of the dominant aging mechanism and state of health (SOH) on the safety of Li-ion pouch cells is investigated. Accelerating rate calorimetry (ARC) is used to determine safety critical temperatures. In order to gain further insights into thermal decomposition processes and enable early detection of critical events, the ARC method is expanded by multiple low-cost sensors installed on and around the pouch cell. Aging associated with Li plating lowers safety by reducing the onset temperature of self-heating (SH), whereas aging at elevated temperatures raises the onset temperature of SH. Typically, temperature is measured on the surface of battery cells during operation or safety testing. However, internal temperature can significantly differ from surface temperature. Therefore, a method is presented in the sixth article that uses laser ablation to insert a thermocouple inside a 21700-type cell. ARC experiments of these cells at different state of charge (SOC) provide insights into thermal gradients. The internal temperature changes much faster and to a greater extent than the surface temperature, especially during venting and thermal runaway (TR). Safety of LIBs is influenced by a number of factors including SOC and aging state. In the seventh article, the safety characteristics of cylindrical 21700-type cells cyclically aged at different temperatures in conjunction with varying SOC are examined by using advanced ARC measurements. The findings indicate that both elevated SOC and cell degradation lower the safety level, both by reducing critical temperatures that necessitate venting and the onset of TR. Furthermore, an increase in destruction level and mass loss of the cell after ARC testing is observed with increasing SOC. Notably, cells exhibiting Li plating show a markedly diminished onset temperature of SH, independent of SOC. Overall, this work provides for the first time comprehensive insights into temperature dependent LIB degradation, with a particular emphasis on the safety of aged cells. These insights are crucial for a safe and efficient operation and can be used to develop improved next-generation LIBs.

Description

Faculties

Fakultät für Naturwissenschaften

DFG Project uulm

EU Project uulm

Other projects uulm

Citation

Is version of

Has version

Supplement to

Supplemented by

Has erratum

Erratum to

Has Part

Kucinskis, G.; Bozorgchenani, M.; Feinauer, M.; Kasper, M.; Wohlfahrt-Mehrens, M.; Waldmann, T. Arrhenius plots for Li-ion battery ageing as a function of temperature, C-rate, and ageing state – An experimental study. Journal of Power Sources 2022, 549, 232129, https://doi.org/10.1016/j.jpowsour.2022.232129
Feinauer, M.; Abd-El-Latif, A. A.; Sichler, P.; Aracil Regalado, A.; Wohlfahrt-Mehrens, M.; Waldmann, T. Change of safety by main aging mechanism – A multi-sensor accelerating rate calorimetry study with commercial Li-ion pouch cells. Journal of Power Sources 2023, 570, 233046, https://doi.org/10.1016/j.jpowsour.2023.233046
Feinauer, M.; Wohlfahrt-Mehrens, M.; Hölzle, M.; Waldmann, T. Temperature-driven path dependence in Li-ion battery cyclic aging. Journal of Power Sources 2024, 594, 233948, https://doi.org/10.1016/j.jpowsour.2023.233948
Waldmann, T.; Hogrefe, C.; Flügel, M.; Pivarníková, I.; Weisenberger, C.; Delz, E.; Bolsinger, M.; Boveleth, L.; Paul, N.; Kasper, M.; Feinauer, M.; Schäfer, R.; Bischof, K.; Danner, T.; Knoblauch, V.; Müller-Buschbaum, P.; Gilles, R.; Latz, A.; Hölzle, M.; Wohlfahrt-Mehrens, M. Efficient Workflows for Detecting Li Depositions in Lithium-Ion Batteries. Journal of The Electrochemical Society 2024, 171, 070526. https://doi.org/10.1149/1945-7111/ad5ef8
Feinauer, M.; Wohlfahrt-Mehrens, M.; Hölzle, M.; Waldmann, T. Unraveling the Complex Temperature-Dependent Performance and Degradation of Li-Ion Batteries with Silicon-Graphite Composite Anodes. Journal of The Electrochemical Society 2024, 171, 110506, https://doi.org/10.1149/1945-7111/ad8d0d
Feinauer, M.; Abd-El-Latif, A. A.; Sichler, P.; Wohlfahrt-Mehrens, M.; Hölzle, M.; Waldmann, T. Effects of Main Aging Mechanism and State of Charge on the Safety of 21700 Li-Ion Battery Cells with Ni-Rich NMC Cathode. Journal of The Electrochemical Society 2024, 171, 110524, https://doi.org/10.1149/1945-7111/ad9356
Feinauer, M.; Hölzle, M.; Waldmann, T. Insights into Thermal Runaway of Cylindrical Lithium-ion Batteries by Internal Temperature Sensors. The Electrochemical Society Interface 2024, 33, 51–54, https://doi.org/10.1149/2.F07243IF

Part of

DOI external

DOI external

Institutions

Periodical

Degree Program

DFG Project THU

EU Project THU

Other projects THU

Series

Collections

Endorsement

Review

Supplemented By

Referenced By

Zeitraum:

Creative Commons license

Except where otherwised noted, this item's license is described as Lizenz A