<link rel="stylesheet" href="styles.cf390c6bfbe7555f.css">

Characterization and analysis of lithium plating on silicon/graphite negative electrodes in lithium ion batteries

Loading...
Thumbnail Image

Date

2024-05-17

Authors

Flügel, Marius

Journal Title

Journal ISSN

Volume Title

Publication type

Document version

Distributor

Universität Ulm

Published in

Abstract

The importance of electric vehicles has increased dramatically with the EU's decision to allow only zero-emission car production from 2035. In addition to powering millions of new cars, electrochemical energy storage systems, i.e. batteries, will also be used for stationary storage of renewable energy in the future. To further improve existing batteries, new materials are being explored constantly, mainly to further increase energy density and to lower specific costs. Silicon (Si) as a new anode active material provides several times the specific capacity of graphite, the most widely used anode active material today, however the aging processes are more severe and therefore more work is necessary to make Si the anode standard in the future. The focus of this work is the occurrence and detection of Li plating on Si/graphite anodes. Better understanding of this phenomena is essential to increase the share of Silicon in graphite anodes without suffering lifetime and safety of such batteries. The energy density of graphite-based Lithium ion batteries (LIBs) correlates with the anode coating thickness. The addition of Si as anode active materials offers the possibility to reduce the anode coating thickness at constant energy density. Based on this finding, three commercial 18650 cells with Si-containing anodes were selected for this work. With these cells as substrates, a new Glow discharge optical emission spectroscopy (GD-OES) method for the quantification of Li deposition on Si/graphite anodes was developed and validated using complementary in-situ and ex-situ techniques. During low temperature cycling ageing, Li plating appeared first in the high energy cells with rather thick and dense anode coating and at lower temperatures also in the high power cell with thinner anodes. The aging mechanism in the first life significantly influences the occurrence of Li plating in the second life aging. Once the mechanism of ageing at 45 °C had been conclusively elucidated, the cells were firstly aged at 45 °C to 80% SOH and then subjected to a second ageing at the conditions that led to Li plating of the fresh cells. In the case of loss of Li inventory (LLI), Li deposition ceased, whereas cells aging by loss of anode active material (LAAM), in this particular case by partial loss of the Si compound, remained susceptible to Li deposition. The second study showed that anodes with higher Si contents and simultaneously lower anode thickness were less susceptible to Li plating. This relationship has been systematically investigated by studying five pilot-scale anodes with different Si contents and very similar areal capacities with respect to Li plating. Cathodes that compensate for the irreversible anode losses with additional areal capacity have been used to build five series of pouch cells with very similar anode capacity despite decreasing anode thickness and fixed N/P ratio. Analysis of the voltage relaxation after charging at different C-rates was used to observe the voltage plateau caused by the re-intercalation of reversibly deposited Li. With increasing Si content and corresponding decrease in layer thickness, the C-rate at which reversible Li plating was firstly detected increases. Ex-situ techniques GD-OES, scanning electron microscopy (SEM), and optical microscopy confirmed these results. Finally, the quantified GD-OES Li depth profiles of four differently aged anodes were validated using neutron depth profiling (NDP). The sputter rate of Li is higher than the carbon (C) sputter rate, which results in a non-uniform sputtering of samples with Li plating on the anode surface. GD-OES and NDP have consistently shown that Li plating occurs only on the anode surface. A new method has been developed which takes into account the changing sputter rate and allows a more accurate depth calculation for samples with Li plating. Due to the higher Li sputter rate, the width of the Li plating peak on the anode surface increases. For aged anodes, the amount of Li irreversibly bound in the anode increases with the degree of aging. The amount of Li in the anode decreases from the surface of the electrode in the direction of the current collector. Due to the high sputter rate of Li, the Li-rich solid-electrolyte interphase (SEI) is preferentially sputtered off, resulting in increased Li detection at the anode surface. The effect of preferential sputtering increases with advanced degree of aging.

Description

Faculties

Fakultät für Naturwissenschaften

DFG Project uulm

EU Project uulm

Other projects uulm

Citation

Has version

Supplement to

Supplemented by

Has erratum

Erratum to

Part of

DOI external

DOI external

Institutions

Periodical

Degree Program

DFG Project THU

EU Project THU

Other projects THU

Series

Collections

Endorsement

Review

Supplemented By

Referenced By

Zeitraum:

Creative Commons license

Except where otherwised noted, this item's license is described as Lizenz A